Impacts of thermal activation on lunar regolith simulant-based precursor and resulting geopolymer: Composition, structure, solubility, and reactivity
G. Xue, G. Qiao | 2025 | Cement and Concrete Composites
DOI 10.1016/j.cemconcomp.2024.105840Simulants: HIT-L-2
Experiments and methods: DSC, Laser diffraction particle sizing, Particle size distribution, XRD, XRF