Primary source
Manufacturing Dense Thick Films of Lunar Regolith Simulant EAC-1 at Room Temperature
Review state
needs review
The film thickness of the investigated cross-section corresponds to the tactile measured thickness of sample 3 (compare Table 3).
Film thicknesses between 2.50 m and 5.36 m have been manufactured obtaining a deposition rate of ~400 m mm 2 /min.