thermal analysis linked to Experiment, with source literature and related extracted records kept visible.
100%
Confidence
2
Literature sources
5
Linked simulants
36
Linked properties
Measurement type
thermal analysis
Application
Experiment
Primary source
Making glass-ceramics from lunar regolith simulant: A study on the crystallization behavior and mechanical properties
Review state
needs review
Differential scanning calorimetry and non-isothermal crystallization kinetics revealed a diffusion-controlled bulk crystal growth with progressively increasing nucleation rates.
the specific heats and thermal diffusivities of LHS-1 and its finer version LHS-1D were studied at low temperatures using differential scanning calorimetry and laser flash analysis.
100%